Product name
Application
Processing & Use level
Characteristics
Low temperature curing accelerator
□ Incorporated into formula before extrusion<br>
□ 0.5-2% by weight of total formula
■ Reduce curing temperature,shorten curing time<br>
■ Improve leveling and anti-yellowing<br>
■ Reduce the gloss fluctuations with curring temperature
Curing accelerator
□ Incorporated into formula before extrusion<br>
□0.05-0.5% by weight of total formula
■ 100% active constituent<br>
■ Reduce curing temperature,shorten curing time
Low temperature curing accelerator
□0.5-1% by weight of total formula
Significantly improve the solvent resistance and impact resistance of the coating film.
Improve the gloss stability of polyester/GMA matting system.
Does not affect leveling and clarity of the coating film.