Product name
Application
Processing & Use level
Characteristics
Charge enhancing agent
□ Incorporated into formula before extrusion
□ 0.3-0.6% by weight of total formula
■ Enhance the conductivity
■ Improve the film appearance
■ Anti yellowing
Charge enhancing agent
□ Incorporated into formula before extrusion
□ 0.2-0.5% by weight of total formula
■ Excellent conductivity performance
■ Improve the film appearance and flow
■ Better overall performance than SA2483
Charge enhancing agent
□ Incorporated into formula before extrusion
□ 0.2-0.4% by weight of total formula
■ Excellent conductivity performance
■ Use for both corona gun and tribo gun
Charge enhancing agent
□ Incorporated into formula before extrusion
□ 0.3-1.5% by weight of total formula
■ No catalytic activity, does not affect the gloss of the coating and the gel time of the coating.
■ Good geothermal stability and anti-yellowing properties.
■ Does not affect powder storage stability.
Charge enhancing agent
□ Incorporated into formula before extrusion
□ 0.3-1.5% by weight of total formula
■ No catalytic activity ,so no negative effect to the gloss of coating and gel time .
■ Good thermal stability and anti-yellowing properties.